The Little Pink Pig – Crawling Glaze

This is a sculpture of a pig that I made when I was much younger. Since I made this piece, my ceramics skills have significantly improved.

However, I still like the sculpture because of its semi-abstract feel. The pink glaze with patches of black slip were used to try and emulate the pattern of the skin of a Gloucester old spot pig. Although, the sculpture did not come out of the glaze firing as I expected, due to “Crawling.”

I have found that this is a problem that is mainly caused by the glaze shrinking too much during the drying process and then inevitably cracking. These cracks then cause crawl points when the clay is fired. This is what you can see on my sculpture where the glaze has split off and almost formed little islands.  

Too much shrinkage of the glaze is usually due to too much raw clay in a glaze. Likewise, if the glaze is applied too thickly, the glaze can still “crawl” .

The more research I have done about Crawling, I think probably the main reason is due to multi-layering different glazes. This is because when you apply more glaze to the clay, the first layer of glaze becomes wet again which in turn affects how the glaze bonds with the clay. As the glaze starts to shrink when it dries, it will start to pull away and crack which means the glaze will then “crawl” during firing.